[FL:4 & 101.6mm]
(1) Ensure that the air cooling is good, otherwise the temperature will be too high and the lens will overheat and crack
(2) There are condensation water drops in the lens barrel, which may cause the lens to break.
(3)The lens is stuck or pollute with the jets of the cut or engrave material, Uneven heating for a long time is easy to cause broken. It should be cleaned with cotton ball dipped in absolute alcohol or acetone in time.
(4) When adjusting the light path, the light path is not correct, the laser accidentally hit the edge of the lens and the junction of the lens barrel, resulting in broken.
Material | PVD Znse |
Wavelength | 10.6μm |
Transmittance | ≥99.5% |
Diameter Tolerance | -0.1mm~-0. 15mm |
Thickness Tolerance | ±0.1mm |
FL Tolerance | <±2% |
Centration | <3 arc minutes |
Clear Aperture | >90% |
Surface Figure | <λ/2 per 1" Dia |
Surface Quality | 40-20 scratch and dig |
AR/AR Coating | R<0.5% per surface |
Compatible Power | 40W-150W |
CO2 laser focus lens is used in CO2 laser engraving/cutting machines.
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
---|---|---|---|---|---|---|
25.4mm/1" | 38.1mm/1.5" | 50.8mm/2" | 63.5mm/2.5" | 76.2mm/3" | 101.6mm/4" | |
Diameter | 12/18/19.05/20/28/25mm | 12/15/18/19.05/20/25mm | 12/15/18/19.05/20/25/30mm | 12/15/18/19.05/20/25/30mm | 12/15/18/19.05/20/25mm | 12/15/18/19.05/20/25mm |
Material | USA CVD Znse/II-VI | USA CVD Znse/II-VI | USA CVD Znse/II-VI | USA CVD Znse/II-VI | USA CVD Znse/II-VI | USA CVD Znse/II-VI |