Use with a rotary device or drill and a polishing pad to restore original glass clarity, and remove blemishes, scuffs, superficial scratches, sanding marks, lime scale, chemical damage and adhesive residue.
|
|
|
---|---|---|
ADD WATERMix 4 parts cerium oxide with 1 part water. Tip! We recommend mixing a small amount of the cerium oxide at a time and adding more if necessary. |
MIXMix by shaking in a closed container or using a spoon/spatula. Tip!: For a more abrasive paste use less water; for a less abrasive paste use more water. |
APPLYApply a small amount (about half a teaspoon) of the mixed cerium oxide compound to a felt pad or similar. |
|
|
|
---|---|---|
START POLISHINGTurn the polishing device on and spread the cerium oxide paste across the damaged area. Tip! Start with low RPM to prevent splatter. |
KEEP POLISHINGIncrease the speed to 1500-2500rpm and polish the area moving side to side or up and down. |
SPRAY WATERWhen the paste dries out, spray a bit of water or add more paste. Keep polishing until you are happy with the results. Tip! For the best experience use a spray bottle with a mist. |
Cerium Fine Grade | Cerium Fine Grade | Cerium Fine Grade | Cerium Fine Grade | |
---|---|---|---|---|
Weight | 1.7 oz (50 grams) | 3.4 oz (100 grams) | 8.4 oz (250 grams) | 1.1 lb (500 grams) |
Costs per Ounce | 6.22 | 4.25 | 2.38 | 1.98 |
Average Particle Size | 2.5 microns | 2.5 microns | 2.5 microns | 2.5 microns |
Purity | TREO 95% | TREO 95% | TREO 95% | TREO 95% |
Suspension Treated | Yes, high water solubility | Yes, high water solubility | Yes, high water solubility | Yes, high water solubility |
Polishing Speed | 1500-2500 RPM | 1500-2500 RPM | 1500-2500 RPM | 1500-2500 RPM |
Contains No Zinc | ? | ? | ? | ? |
Color | White | White | White | White |
Packaging | PET Jar | PET Jar | PET Jar | Plastic Bag |